Parameter:
Items
|
Units
|
Measurement Indicators
|
Measurement Results
|
Compressive Strength
|
%( of the benchmark
of mortar strength)
|
28d≥75%
|
117%
|
Coursing Degree
|
mm
|
10---30
|
16
|
Air Content
|
%
|
≤20
|
8
|
Difference in Setting Time
|
min
|
+60---- -60
|
+23
|
Cohesive Strength
|
MPa
|
≥0.2
|
0.4
|
Brief Introduction:
Architectural masonry and plastering additives for aerated blocks consists of
polymer and several high-efficient additives. It has good cohesive strength, water
retention and crack resistance so it makes sure of best cohesive performance
of aerated blocks.
Features:
1. Good water retention, strong cohesive strength, and high compressive strength so it makes aerated blocks with good cohesive strength, good frost-resistance, safety, non-cracks and non-crack-hollows.
2. Good workability, convenient to use in construction, speed up construction efficiency.
3. Time-saving, energy-saving, economical and practical, durable, and environmental safety.
Usage Range:
It can be used in architectural masonry mortar and plastering mortar for all kinds of coal ash and aerated blocks.
Reference Mixture Ratio:
The mixture ratio of agent to cement is 0.5%--0.7%, and here is a measurement spoon in every pack.
Usage:
1. Mixing procedure while using vertical mixers, horizontal mixers: Firstly, mix part sand, agent and water and stir them uniformly. Put cement and all sand into them. At last, stir the mixture for 3~5 minutes.
2. Mixing procedure while using drum-type mixers: Put agent, cement, and sand together, stir them for 1 minute. And then add water to the mixtures and stir for 3~5minutes.
3. Artificial mixing: the agent should be first dissolved into the water then placed into mortar.
4. The first mixing mortar, the quantity of agent should be increased 1 time.
5 The water in the mortar with the agent should be reduced by 20%.
6 The mixture ratio of agent fluctuates with different cement and sand. So the reasonable ratio should be depended on the materials at the site and trial.